TDI/PPG PU Prepolymer System For PU Scrapers 1. Application: It can be used to make rods, caster wheels, rollers, Sealing rings, sieve plates and ...
2024-12-09 19:23:09
|
|
TDI/Polyester Polyurethane Preploymer Hardness 92 1. Description This is a TDI-terminated PET prepolymer of low viscosity and easy processing. It ...
2024-12-09 22:37:18
|
|
...80 is a mixture of 80% 2,4-toluene diisocyanate and 20% 2,6-toluene diisocyanate. It is mainly used in the preparation of flexible polyurethane ...
2024-12-26 08:34:14
|
|
TDl / Polyester Polyurethane Preploymer Hardness 72 1. Description This is a TDI-terminated PET prepolymer of low viscosity and easy processing. It ...
2025-03-05 14:22:15
|
|
TDl / Polyester Polyurethane Preploymer Hardness 60 1.Description This is a TDI-terminated PET prepolymer of low viscosity and easy processing. It ...
2024-12-09 22:49:11
|
|
TDl / Polyether Polyurethane Preploymer Hardness 70 1.Description This is TDI-terminated PPG prepolymer of low viscosity and easy processing. It ...
2024-12-09 22:49:11
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 280-300 4.50-4.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ...
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 280-300 5.00-5.20 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ...
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 350-370 4.50-4.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ...
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 210-230 5.00-4.20 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ...