Detailed Product Description
MDI/Polyether Polyurethane Prepolymer Shore A80 1. Description
This is a MDI based polyether polyurethane prepolymer.
2. Characteristics
3. Applications
4. Typical properties
5. Operating Procedure
First, the prepolymer should be preheated in 80-85℃. Second, after vacumming, the prepolymer is to be mixed with melting MOCA evenly. Third, with degassing, casting into mould, and vulcanization,and then demould. Lastly, the finished product should be post vulcanized.
6. Reaction parameters
7. Finished products properties
|
||||||||||||||||||||||||||||||
Product Tags: Odorless MDI Polyether Polyurethane Shore A80 MDI Polyurethane A80 MDI Polyether Polyurethane |
Related Products
![]() |
MDI / Polyester Prepolymer ME1685 Equivalent To Erapol EME85A |
![]() |
White Solid MDI/PTMG Prepolymer Hardness 95 |
![]() |
White Solid MDI / PTMG Based Prepolymer Abrasion Resistant Hardness 90 |
![]() |
White Solid MDI / PTMG Prepolymer Hardness 85 For PU Rods |
![]() |
White Solid MDI/Polyester Prepolymer Hardness 95 |
![]() |
White Solid MDI / Polyester Prepolymer Hardness 90 For PU Rods |
Email to this supplier