Low Free TDI/Polyester Prepolymer (LFE4390) Product Specification Product Type LFE4390 Batch No. 20250220 Production date 2025/2/20 Test Item Test ... 2025-10-22 09:05:32
Low Free TDI/Polyester Prepolymer (LFE3382) Product Specification Product Type LFE3382 Batch No. 20250220 Production date 2025/2/20 Test Item Test ... 2025-10-22 09:05:32
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 300-330 6.50-6.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Solid 1100-1200 5.00-5.20 20/200 5. Operating Procedure First, the prepolymer should be 2024-12-09 19:23:09
TDI-100/PTMG Polyurethane Prepolymer Shore A95 1. Description This is a TDI-100 based PTMG polyurethane prepolymer. 2. Characteristics Water ... 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Solid 1200-1300 3.00-3.20 20/200 5. Operating Procedure First, the prepolymer should be preheated in 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 250-270 5.50-5.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 300-330 4.50-4.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 200-250 2.80-2.95 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Solid 900-1000 5.00-5.20 20/200 5. Operating Procedure First, the prepolymer should be preheated in 2024-12-09 19:23:09