TDI/PPG PU Prepolymer System For PU Scrapers 1. Application: It can be used to make rods, caster wheels, rollers, Sealing rings, sieve plates and ...
2024-12-09 19:23:09
|
|
...80 is a mixture of 80% 2,4-toluene diisocyanate and 20% 2,6-toluene diisocyanate. It is mainly used in the preparation of flexible polyurethane ...
2024-12-26 08:34:14
|
|
TDl / Polyether Polyurethane Preploymer Hardness 70 1.Description This is TDI-terminated PPG prepolymer of low viscosity and easy processing. It ...
2024-12-09 22:49:11
|
|
.... It has excellent processing properties, solid in common temperature, shorter gel time, and regulating colour by adding pigment. The ware has good ...
2025-10-22 09:05:36
|
|
..., etc. 3. Product Specification NCO Content (%) 7.5±0.2 Density (25℃)/(g/cm3) 1.11 Viscosity at 85℃ (Mpa.s) 1000 Appearance at 25℃ White solid 4....
2024-12-09 22:52:57
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 280-300 4.50-4.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ...
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 280-300 5.00-5.20 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ...
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 350-370 4.50-4.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ...
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 210-230 5.00-4.20 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ...
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 400-420 5.30-5.50 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ...
2024-12-09 19:23:09
|