Selling leads
...(mPa.s/85℃) NCO% Packing(kg/drum) Solid 1100-1200 5.00-5.20 20/200 5. Operating Procedure First, the prepolymer should be 2024-12-09 19:23:09
...Polyurethane Prepolymer Shore A95 1. Description This is a TDI-100 based PTMG polyurethane prepolymer. 2. Characteristics Water resistance Low ... 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Solid 1200-1300 3.00-3.20 20/200 5. Operating Procedure First, the prepolymer should be preheated in 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 250-270 5.50-5.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 300-330 4.50-4.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 200-250 2.80-2.95 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Solid 2200-2400 3.00-3.20 20/200 5. Operating Procedure First, the prepolymer should be 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 280-300 4.50-4.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ... 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 280-300 5.00-5.20 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ... 2024-12-09 19:23:09
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 350-370 4.50-4.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃. ... 2024-12-09 19:23:09