Machine Parts Polyester Based Polyurethane Shore A80
|
Detailed Product Description
|
TDI-100/Polyester Polyurethane Prepolymer Shore A80 1. Description
This is a TDI-100 based Polyester polyurethane prepolymer.
2. Characteristics
3. Applications
4. Typical properties
5. Operating Procedure
First, the prepolymer should be preheated in 80-85℃. Second, after vacumming, the prepolymer is to be mixed with melting MOCA evenly. Third, with degassing, casting into mould, and vulcanization,and then demould. Lastly, the finished product should be post vulcanized.
6. Reaction parameters
7. Finished products properties
|
||||||||||||||||||||||||||||||
| Product Tags: Machine Polyester Based Polyurethane Machine Parts Polyester Polyurethane Shore A80 Polyester Based Polyurethane |
Related Products
|
TDI / PTMG Prepolymer E3695 Equivalent To Erapol E95A |
|
TDI / PTMG Prepolymer E3382 Equivalent To Erapol E83A |
|
TDI / PTMG Prepolymer E3490 Equivalent To Erapol E90A |
|
Shore A90 TDI 100 Polyurethane Prepolymer |
|
TDI Polyester Polyurethane Preploymer Hardness 72 shore A |
|
TDl / Polyester Polyurethane Prepolymer Hardness 96 |
Email to this supplier