MP35N Alloy Wire Nickel Based Alloys With Excellent Ductility And Toughness
|
MP35N alloy wire Diameter 1.5mm/3mm AMS 5844 260 to 300 ksi (1793-2086 MPa)
MP35N alloy wire is a non-magnetic nickel cobalt chromium molybdenum alloy, which has unique ultra-high tensile strength (up to 300ksi [2068mpa], good ductility, toughness and very good corrosion resistance. In addition, the alloy also exhibits outstanding resistance to vulcanization, high temperature oxidation and hydrogen embrittlement. The unique properties of mp35n are obtained by work hardening, phase transformation and aging treatment. If the alloy is used under full work hardening conditions, the recommended temperature is 750 ° f (399 ° C) with an operating temperature of - 200-315 ° C.
3, Purpose of mp35n:
Mp35n alloy can be used for fasteners, springs, non-magnetic components and instrument components in medical, seawater, oil and gas wells, chemical and food processing environments.
4, Corrosion resistance:
Mp35n has good properties of anti sulfurization, high temperature oxidation, brittleness, salt spray and most mineral acids. The alloy has the ability to resist stress corrosion cracking under severe environment and high strength. The alloy also has high resistance to local corrosion, such as pitting and crevice corrosion.
5, Room temperature strength:
The yield strength of mp35n can reach 1999 MPa
MP35 N wire specification Φ 0.03m/m ~ Φ 12m / M delivery status: spring hard wire (tensile strength ≥ 1400MPa), acid white / hydrogen soft wire, fine wire delivery, round steel (hot rolling or solid solution delivery)
Characteristics of MP35N alloy:
· Chemical composition:
MP35N Physical propertie
The minimum mechanical properties of MP35N alloy at room temperature:
the microstructure, monotonic, and cyclic response of as drawn ~100 μm diameter MP35N low-Ti alloy wire were presented and discussed. In this sequel paper, the effects of annealing the same cold-drawn wire on microstructure and mechanical properties are examined. Specifically, segments of the wire were annealed for 1 h at 973 K, 1023 K, 1073 K, 1123 K and 1173 K in a vacuum furnace. .
|
|||||||||||||||||||||||||||||||||||||||||||||||||
Product Tags: ni based superalloys nickel based superalloys |
![]() |
High Magnetic Flux Soft Magnetic Alloy Plate 1J22 Plate |
![]() |
High Coefficient Of Thermal Expansion Co50V2 1J22 Permalloy Plate |
![]() |
Kovar Alloy 4J29 Plate Invar 4J32 4J33 4J34 4J36 Sheet |
![]() |
UNS K94610 Kovar Alloy Bar With Good Low Temperature Tissue Stability |
![]() |
4j29 Kovar Alloy Wire Fe-Ni-Co Glass Sealing |
![]() |
Hastelloy C276 Welding Wire c276 welding wire hastelloy c276 welding rod |