Selling leads|
TDI-terminated PPG Prepolymer – Low Viscosity Polyurethane Prepolymer This TDI-terminated PPG prepolymer features low viscosity, easy processability, ...
2026-04-10 07:30:19
|
|
Wear Resistance Skate Wheel TDI/Polyester Based Polyurethane Prepolymer Polyurethane is a good match for the wheel since various polyols and ...
2024-12-09 19:23:09
|
|
... and important basic raw materials. The commonly used TDI in the polyurethane industry is a mixture of 2,4-TDI and 2,6-TDI isomers, including 3 ...
2024-12-09 19:42:22
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Solid 1200-1300 3.50-3.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in
2024-12-09 19:23:09
|
|
TDI-100/PTMG Polyurethane Prepolymer Shore A95 1. Description This is a TDI-100 based PTMG polyurethane prepolymer. 2. Characteristics Water ...
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Solid 1200-1300 3.00-3.20 20/200 5. Operating Procedure First, the prepolymer should be preheated in
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 250-270 5.50-5.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃.
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 300-330 4.50-4.70 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃.
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 200-250 2.80-2.95 20/200 5. Operating Procedure First, the prepolymer should be preheated in 80-85℃.
2024-12-09 19:23:09
|
|
...(mPa.s/85℃) NCO% Packing(kg/drum) Liquid 400-500 5.00-5.20 20/200 5. Operating Procedure First, the prepolymer should be