Polyurea Special Waterborne Polyurethane Surface Coating SQM-A01/B02

Brand Name EXCEEDCHEM
Model Number SQM-A01/B02
Certification ISO9001:2008
Place of Origin China
Minimum Order Quantity 1mt
Price FOB Qingdao usd4.9/kg
Payment Terms L/C, T/T
Supply Ability 3000mt/month
Delivery Time 5-8 work days
Packaging Details component A (main agent) 18.75kg component B (curing agent) 1.25kg
Product name Polyurea special waterborne polyurethane surface coating
Suggested thickness of the dry film layer 150-200 μ m
Apply to PVC, polyurea, silicon PU
Water resistance (25℃ tap water) No change in 30 days
Surface gloss semi-light
Component two
Detailed Product Description

Polyurea special waterborne polyurethane surface coating SQM-A01/B02

Characteristics

  • high hardness, strong scratch resistance, has a certain flexibility
  • No solvent, no pollution, non-toxic harm
  • Resistance to acid, alkali and chemicals
  • Wear resistance, pressure resistance, high temperature resistance, yellowing resistance, waterproof and moisture-proof, fire prevention and other comprehensive performance is the best

Scope of Application

suitable for PVC, silicon PU, polyurea and other base surface, to provide good strength and adhesion.

 

Application Place

laboratory, research and development room, pharmaceutical factory, cigarette factory, subway station, railway station, schools, hospitals, airports, passenger transport center and other public places

 

Typical characteristic

Adhesion1
Abrasive resistancegreat
Water resistance (25℃ tap water)No change in 1 month

 

Basic parameter

Surface glosssemi-light
Componenttwo
Suggested thickness of the dry film layer150-200 μ m
Water resistanceNo change in 30 days

 

 Construction instructions

Apply toPVC, polyurea, silicon PU
Construction methodtraditional spraying, rolling coating
Mixing ratio, weight ratioA: B=15:1 (Construction after 5 minutes of mixing)

 

 

Drying time

The substrate temperatureSurface drying timeReal dry
(℃)(H)(H)
15-25224

 

 

Packaging specification

component A (main agent) 18.75kg component B (curing agent) 1.25kg

 

Product Tags: SQM-A01 / B02 Polyurea surface coating   Polyurea surface coating   Polyurea special waterborne polyurethane surface coating  