Hastelloy C Is A Nickel-Chromium-Molybdenum Alloy With Excellent Resistance To Oxidation And Corrosion Hastelloy C Alloy is a high-performance nickel...
2025-07-31 00:28:28
|
... 0.5-1.5% 0.15-0.25% 0.6% Trace elements such as manganese (Mn), silicon (Si), phosphorus (P), and sulfur (S) are also included. Physical ...
2025-07-31 00:28:28
|
...Resistant Hastelloy C276 Hastelloy Plate Nickel-based Alloy Steel Plate 2-60mm. C276 Hastelloy, also known as Inconel C276, is a high-performance ...
2025-07-31 00:28:28
|
Incoloy 925 Alloy: High-Strength, Corrosion-Resistant Nickel-Iron-Chromium Alloy For Demanding Applications Product Description of Incoloy 925 Alloy: ...
2025-07-31 00:28:28
|
...Nickel-Based Alloy 625: chemical composition: Alloy % Ni Cr Mo Nb Fe Al Ti C Mn Si Co P S Inconel 625 maximum margin 20 8 3.15 - - - - - - - - - ...
2025-07-31 00:28:28
|
... wear resistance, hardness, and corrosion resistance. It is particularly effective in environments subject to high temperatures and abrasive ...
2025-07-31 00:28:28
|
Alloy 30: Advanced Alloy With Superior Corrosion Resistance For Demanding Industrial Applications Alloy 30 Product Description: Alloy 30, also known ...
2025-07-31 00:28:28
|
...18.0% chromium, 24.0-26.0% nickel, and 4.5% molybdenum. 904L Super Austenitic Stainless Steel is a low-carbon, high nickel, molybdenum austenitic ...
2025-07-31 00:28:28
|
Incoloy 825 Alloy: High-Performance Nickel-Iron-Chromium Alloy For Corrosive Environments Product Description of Incoloy 825 Alloy: Incoloy 825 is an ...
2025-07-31 00:28:28
|
... 800H and 800HT are normally used in temperatures above 1100° F where resistance to creep and rupture is required. The chemical balance allows the ...