1j50 soft magnetic alloys strip

Selling leads
Soft Magnetic Alloys Strip 1J50/ Ni 50 Ni-Fe soft magnetic alloy strip Mainly used in two areas for energy conversion and information processing In ... 2026-05-31 00:04:59
1J50 50Ni-Fe(Square Orthonol / Permenorm 5000 Z) Chemical Composition:(%) Name Ni Fe Mn Si C 1J50 50Ni-Fe (Permenorm 5000 Z) 49-51 Balance 0.30-0.60 0... 2026-02-12 00:24:12
Soft Magnetic Alloys Strip 1j85 / E11c / Ni80mo5 / 1j79 / Mu 80 Permalloy for Transformer Core Permalloy Permalloy is a nickel-iron, soft magnetic ... 2024-12-09 13:03:33
... elements. It is characterized with a fixed coefficient of expansion. Increase the thermal expansion coefficient and the Curie point with increase ... 2024-12-09 13:03:42
Chemical composition composition C P S Mn Si ≤ Content(%) 0.03 0.02 0.02 0.6~1.1 0.3~0.5 composition Ni Cr Mo Cu Fe Content(%) 78.5~80.0 - 3.8~4.1 ≤0... 2024-12-09 11:43:20
... induction and low core loss of the alloy. In the electronics industry, mainly at low or medium alloy having a high magnetic permeability and low ... 2025-04-24 08:33:28
...Soft Magnetic Alloy High Permeability 1J22 1J50 1J79 1J85 Precision Alloys: Precision Alloys have special physical and mechanical properties, and ... 2024-12-09 11:22:33
... of most varieties and specifications, dosage after silicon steel sheet and electrical pure iron.Compared with other soft magnetic alloy, the alloy ... 2024-12-09 11:46:58
...1j50 Carbon Content Less Than 0.03% Diameter 0.1~10mm Condition Soft/ Hard Surface Bright/ Dard Linear expansion coefficient 9.20 resistivity 0.45 ... 2025-03-11 19:31:26
...saturation induction 0.65-0.75 T. Alloy 1J79/ permally high squareness of the hysteresis loop and a low coefficient of magnetization reversal ... 2024-12-09 12:31:54