... , colorful Width 90cm , 100 cm , 150cm Weight 25 gsm Coating method Double dot Adhensive PA Fusing Temperature (Roller) 125 ~ 135 ℃ Pressure 2.0 ~ ...
2025-03-27 00:32:21
|
...Woven Fusible Interlining PA Coating For Garments Detailed Description: TECHNICAL SPECIFICATION SHEET N8208 Composition 20% Polyester , 80% Nylon ...
2025-03-27 00:32:22
|
... 90cm , 100 cm , 150cm or cutting to tape Weight 43 gsm Coating method Double dot Adhensive PA Fusing Temperature (Roller) 125 ~ 135 ℃ Pressure 2.0 ...
2025-03-27 00:32:22
|
...Woven Interlining With Nylon / Polyester Composition Detailed Description: TECHNICAL SPECIFICATION SHEET N5368S Composition 50% Polyester / 50% ...
2025-03-27 00:32:24
|
...Woven Interlining N8371S With Double Dot Pa Coating Detailed Description: TECHNICAL SPECIFICATION SHEET N8371S Composition 20% Polyester / 80% ...
2025-03-27 00:32:24
|
... 80 cm , 92 cm , 102 cm Weight 37 gsm Coating method Scatter coating Adhensive LDPE Fusing Temperature (Roller) 125 ~ 140 ℃ Pressure 1.0 ~ 2.0 Time ...
2024-12-09 11:10:33
|
... , Black Width 122 cm , 150cm Weight 54 gsm Coating method Double dot Adhensive PA Fusing Temperature (Roller) 130 ~ 150 ℃ Pressure 2.0 ~ 4.0 Time ...
2024-12-09 11:22:17
|
...Woven Interlining For Men's Suit Heavey Fabric T7308 - 100 Detailed Description: TECHNICAL SPECIFICATION SHEET T7308 - 100 Composition 100% ...
2024-12-09 11:22:17
|
...Woven Interlining For Men And Women ' s Trousers 3272 Detailed Description: TECHNICAL SPECIFICATION SHEET 3272 Composition 80% polyester / 20% ...
2024-12-09 11:27:42
|
... 90cm , 100 cm , 150cm Weight 40 gsm Coating method Single dot Adhensive PA Fusing Temperature (Roller) 125 ~ 140 ℃ Pressure 2.5 ~ 3.0 Time 13 ~ 15 ...