0.18 - 2.5 mm Thickness Aluzinc Coated Steel , Hot - Dip GL Sheet
For Appliances Profile : Galvalume Steel Is Tthe Plating Coat Of Aluminum-zinc Alloy Armor
Plate,And Its Composition Is 55 % Al , 43.4 % Zn And 1.6 % Si . The
Plate With Smooth Surface And Excellent Corrosion Resistance Of The
Atmosphere , Which Is 2 To 6 Times Higher Than Hot-Dip Galvanized
Sheet Of The Same Thickness Of Coating . Specifications of Aluzinc Coated Steel : ■Standard : ASTM A792 / JIS G3321 / GB / T14978 - 2008 / EN10326 -
2004 ■Grade : SGLCC / SGLCD / SGLC400~570 / DC51D + AZ ~ DC54D + AZ ■Thickness : 0.15-2.5 mm ■Width : 600 - 1250 mm ( Usually 914 mm / 1219 mm / 1220 mm / 1250
mm) ■Base Metal : Cold - Rolled Steel ■Al-Zinc Coating : 50 - 150 g / sqm ■Coil Internal Diameter : 508 mm / 610 mm ■Surface Treatment : Chromate Passivated , Non - Chromate
Passivated , Oiled , Anti - finger Print And Etc ■tolerance thickness : + / - 0.05 mm , tolerance width : + 5 / - 2
mm , total quantity : + / - 10 % , alu - zinc coating : + / - 10 % ■Packing Condition : Seaworthy Characteristics : GL are 3 ~ 6 times more corrosion - resistant compared to GI , but
has a similar level of processability and weldability and can
replace GI, and in particular is most suitable when replacing GI
that require thick galvanized layers and high corrosion resistance
. Only galvanized steel sheet that is used for roofing and walls
without painting because of its unique silver spangles and
beautiful appearance and high - corrosion resistance, and is used
as a cool roofing material because of its excellent heat reflection
qualities . Can replace aluminum gilded steel sheets because for certain
purposes of its electrical conductivity and its heat-resistance
qualities even at high temperatures that do not exceed 315 ℃ . Has greater surface hardness than GIs , and is much more wear -
resistant . Corrosion resistance increased more with resin-coating treatment ,
which enables roll forming or press forming without the spraying of
processed oils . Application of Aluzinc Coated Steel : Infrastructure : Roofing / External Siding / Garage / Shutter Household Appliances : Oven / Air - Conditioning Ventilation System
/ Solar Water Heater / Electronics Automobile : Mobile Muffler / Vent Pipe / Catalysis Converter
Heater Shield / Bottom Accessories Industrial Instrument : Electric Control Cabinet / Industrial
Freezer Chest
Chemical Requirements : Chemical Requirements For Structure Steel | Composition , % - Heat Analysis Element , Maximum , Unless
Otherwise Shown | Designation | C | Mn | P | S | Cu | Ni | Cr | Mo | V | Cb | Tia | Nb | G230 | 0.20 | 1.35 | 0.04 | 0.04 | 0.25 | 0.20 | 0.15 | 0.06 | 0.008 | 0.008 | 0.025 | * | G255 | 0.20 | 1.35 | 0.10 | 0.04 | 0.25 | 0.20 | 0.15 | 0.06 | 0.008 | 0.008 | 0.025 | * | G275 | 0.25 | 1.35 | 0.10 | 0.04 | 0.25 | 0.20 | 0.15 | 0.06 | 0.008 | 0.008 | 0.025 | * | G340 | 0.25 | 1.35 | 0.20 | 0.04 | 0.25 | 0.20 | 0.15 | 0.06 | 0.008 | 0.008 | 0.025 | * | G550 | 0.20 | 1.35 | 0.04 | 0.04 | 0.25 | 0.20 | 0.15 | 0.06 | 0.008 | 0.015 | 0.025 | * |
|