High Mn imbedding cemented carbide hammer Inlaid Alloy Hammer
alloy steel hammer
The alloy steel material that be crushed by hammer crusher is a
tremendous difference. The crusher has different forms and hammers.
In the condition of crush hard and tough material such as iron raw,
Our high Cr bimetal hammer could bear the cutting from the material
but easy be come off or break for the hammer’s toughness property
is not good. Though the toughness of supper Mn steel is higher but
the wear resistant property is not enough. So hammer and blow bar
made from high Mn imbedding cemented carbide is the best choice.
The High Mn imbedding cemented carbide hammer(Inlaid Alloy Hammer /
alloy hammer/hammer mill) product made by our company use the wear
resistant bar made from higher content nano-sized tungsten carbide
and titanium carbide. The Rockwell hardness of wear resistant bar
is 80HRA~90HRA. We will make the hammer’s matrix with high Mn or
super high Mn according to the complexity of hammer mill. We make
sure of the 100% metallurgical bonding of the alloy steel material
bar surface and matrix by the method of blowing argon at bottom of
furnace, diversified qualitative change, diversified inoculation,
and appropriate casting, smelting, heat treating.These processing
measure increase the combination property of the High Mn imbedding
cemented carbide products made by our company. This kind of alloy
steel material hammer is widely used in hammer mill. We meet with
great favor from our customers at home and abroad.
Specifications:
Standard | Chemical component % |
C | Mn | Si | Cr | S | P |
ZG120Mn13Cr2 | 1.05~1.35 | 11~14 | 0.3~0.9 | 1.5~2.5 | ≤0.04 | ≤0.04 |
ZG120Mn17Cr2 | 1.05~1.35 | 16~19 | 0.3~0.9 | 1.5~2.5 |
Notes:Allowed to join trace V,Ti,Ba and RE and so on. |
The mechanical properties of the matrix:
Standard | Lower yield strength Rel MPa | Tensile strength Rm Mpa | The section elongation A% | Shock absorption KU2 J | Hardness HBW |
ZG120Mn13Cr2 | ≥390 | ≥735 | ≥20 | — | ≤300 |