High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator
|
|
High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator
Quick Detail:
Description:
Chemical composition(%)
Physical properties >Density (g/cm3): 8.4 >Melting point (℃): 1370~1425
Mechanical properties
Specifications
|
|||||||||||||||||||||||||||||||||||||||||||||||||||||||||