Screen Printing Ink
Overprinting
Please bear in mind that the ink film underneather is not chemically cured when first
overprinted.If the ink film is dried at room temperature
20℃,overprinting must be carried out with hardener PUH in the
course of 12 hours and with hardener PEMH in the course of 8 hours
at the lates.We recommend to carry out the overprinting as soon as
possible,in order to guarantee good adhesion between the ink
layers.
Stress resistance
After proper and thorough drying(20℃-8days),the ink film exhibits
outstanding adhesion as well as rub and scratch resistance and is
resistant to most usual fillers(slightly alkaline to acid),as well
as to alcohol,oils,greases,finger sweat,petrol,battery acid,and
other solvents.In general,the chemical resistance of PU is improved
by heat forced drying,e.g 150℃ for 30 min.If hardener HT1 is
used,oven drying is essential.
Application:
Marapur PU is a versatile and highly resistant two-component ink
which is applicable in all cases where highest demands for chemical
and mechanical resistance for indoor and outdoor use have to be
met.PU is also designed for printing onto polyolefines(PE,PP),the
substrate's surface has to be pre-treated as usual by flaming or
Corona-discharge.This increases the surface tension,and a
sufficient adhesion can be achieved with a minimum surface tension
of 42-48 mN/m.PU can also be processed with a spray gun,but
preliminary trials are necessary for this process.We recomment to
filter the thinned ink(25 μm screen)before processing,as otherwise
there could be bubbles in the ink film